Technical Parameter | |
Hardness After Hardening&Tempering | HB280-320 |
Nitride Haedness | HV850-1000 |
Nitride Brittleness | Less than Grade Two |
Surface Roughtness | Ra 0.4 |
Screw Straightness | 0.015mm |
Alloy hardness | HRC50-65 |
Alloy depth | 0.8-2.0mm |
Surface Chromium-Plating’s Hardness After Nitriding | More than 900HV |
Chromium-Plating Depth | 0.025-0.10mm |
Packaging | Wrapped in Film by wood case |
Payment | T/T L/C western union |
Delivery time | 25 days |
Harbor | Ningbo/Shanghai |
Lifespan | More than 2 years |
Processes |
Bimetal Spraying Process Corrosion &Abrasion Resistance |
Advanced Gas Nitride Process |
Centrifugal Casting |
Cold/Thermal Spray Hard Metal Process |
Materials |
38CrMOAlA ( JIS SACM645) |
42CrMo (JIS SCM440) |
40Cr |
GH113 |
SKD11 |
SKD61(H13) |
Gr12MoV |
Duplex Stainless Steels
|