It is made of used butyl inner tires and butyl capsules, refined and without grains, applicable for manufacture of butyl inner tires, butyl capsules, other rubber products that airtight nature , able to bear the high-temperature rubber products and so on.
The Chemical and Physical Property Index of Refined Butyl Reclaimed Rubber:
Item\Index\ Species,Grade | Water content | Ash content | Extraction of acetone | Density | Stretch strength | Elongation rate | Menni | |
% ≤ | % ≤ | % ≤ | g/cm3 | MPa ≥ | % ≥ | ML(100°C,1+4) ≤ | ||
Inner Tire | Excellent | 0.5 | 6 | 10 | 1.2 | 11 . 0 | 490 | 40 ~ 50 |
First Grade | 0.5 | 8 | 15 | 1.2 | 8.0 | 480 | 50 ~6 0 | |
Capsule | Excellent | 0.8 | 8 | 15 | 1.2 | 10. 0 | 480 | 50 ~6 0 |
First Grade | 0.8 | 10 | 18 | 1.2 | 7.0 | 460 | 60 ~7 0 |