CONDENSATION CURE RTV-2 MOLDMAKING SILICONE
Product | Catalyzed Viscosity: cps | Base Color | Specific Gravity | Mixed Ratio | Shore A Hard | Tensile (Map) | Elongation % | Tear KN/m |
RTV M20 | 20,000 | Beige | 1.25 | 100:2 | 20-22 | >2.8 | >500 | >2.0 |
RTV M25 | 21,000 | Beige | 1.25 | 100:2 | 25-26 | >3.0 | >480 | >2.5 |
RTV M30 | 30,000 | Beige | 1.21 | 100:2 | 30-32 | >3.8 | >460 | >2.8 |
RTV 330 | 35,000 | Translucent | 1.28 | 100:2 | 30-32 | >3.8 | >460 | >3.0 |
[1] Application of silicon rubber for statues mold
Silicon rubber for statues mould is mainly applicable to make the silicone mould for cultural relic duplication, architectural decoration, resin crafts, lighting ornaments, candles, statues, model design, product exploitation, etc.
[2] Features of silicon rubber for statues mold:
Silicon rubber for statues mould is generally named two -component room temperature vulcanization silicone rubber, a kind elastic silicone rubber mold which features with resistance to deformation, high-temperature, acid-alkali and expansion.
[3] Instruction of silicon rubber for statues mold:
Silicon rubbers for statues mould are generally named as two-part room temperature sulfur Ted silicone rubber, which features an exceptional fluidity and good operability.When mixed with 2-3% curing agent, they can still be operated within 30 minutes, but will be formed after 2-3 hours.With resistance to deformation, high temperature, acid and alkali, and expansion, silicon flexible molds are used for mold duplication and delicate mold making for polio crafts, resin crafts lighting and candle crafts.
[4]Frequently asked questions of silicon rubber for statues mold.
Why does the mold made of silicone rubber have an unsmooth surface with tracks and strips on it?
It is due to product or model to be molded should have been sanded or polished. If the mold or product is not sanded or polished, the mold made of whatever quality silicone rubber will not be good and smooth enough since the mold or the product itself is not smooth or perfect. Another case is that uneven brushing of the release agent will also bring about uncouthness of the mold.
We can provide you the best quality rtv silicone rubber with competitive price and free remold technology.
Any question ,please feel free to contact MS Betty Xu
TEL:0086-755-27052112
FAX:0086-755-27052562
Mobile:0086-15814448960
skype:betty8980