CONDENSATION CURE RTV-2 MOLDMAKING SILICONE
Product | Catalyzed Viscosity:cps | Base Color | Specific Gravity | Mixed Ratio | Shore A Hard | Tensile (Mpa) | Elongation % | Tear KN/m |
RTV M20 | 20,000 | Beige | 1.25 | 100:2 | 20-22 | ≥2.8 | ≥500 | ≥2.0 |
RTV M25 | 21,000 | Beige | 1.25 | 100:2 | 25-26 | ≥3.0 | ≥480 | ≥2.5 |
RTV M30 | 30,000 | Beige | 1.21 | 100:2 | 30-32 | ≥3.8 | ≥460 | ≥2.8 |
RTV 330 | 35,000 | Translucent | 1.28 | 100:2 | 30-32 | ≥3.8 | ≥460 | ≥3.0 |
1) RTV molds making materials silicone rubber applications
RTV molds making materials silicone rubber is primarily intended for poly resin crafts, PU crafts, PU resin crafts ,gypsum crafts ,unsaturated resin crafts, lighting and candles crafts ,plastic toy , stationery gifts crafts industry, a large statue Buddha, relievo ,furniture, furniture decorative materials, statues Buddha, artifacts copied, building decoration materials, large-scale cement mold, artificial fossils Factory, Europe component factory, simulation landscapes, animals and plants sculpture, sandstone crafts and so on.
2) RTV molds making materials silicone rubber features description
RTV molds making materials silicone rubber is white or red flowing liquid with general hardness of 22-50A°after curing. Molding silicone is a kind elastic silicone which features with resistance to deformation, high-temperature, acid-alkali and expansion as well as high reproduction times, good tensile strength, tear strength and elongation.
3) RTV molds making materials silicone rubber operations
If the customer wants to make large products and large size molds, the mold should be made of silicone material with high hardness. On the contrary, if the mold with fine and precision patterns, it should be made of silicone materail with low hardness. The amount of the curing agent depends on the actual requirements of the customer. If molds requiring fast drying and demold, more curing agent is needed; contrarily, if molds requiring slower drying and demold, less curing agent is needed.
(Notes: our company does not recommend you to add silicone oil. If a special soft silicone materail mold or fine detailed and complex patterns products are required, 5%-10% silicone oil can be added to soften the mold for easy demold.)
Frequently asked questions of RTV molds making materials silicone rubber
Why does the silicone mold have few molding times?
The silicone rubber mold has few molding times is due to follwoing reasons: adding too much silicone oil which will destroy the molecular of silicone material ; making the mold for small and fine detailed products with higher hardness silicone material which is easy to break; making the mold for large products with soft silicone materail which will reduce the tensile and tear strength of the mold, and the mold will have deformation. Thus, we should take the proper silicone rubber to make the mold for suitable products
We can provide you the best quality rtv silicone rubber with competitive price and free remold technology.
Any question ,please feel free to contact MS Betty Xu
TEL:0086-755-27052112
FAX:0086-755-27052562
Mobile:0086-15814448960
skype:betty8980
Website:www(dot)lhsilicone(dot)com