1.Spolit fire bricks, magnesite chrome brick
2.Good high temperature properties
3.Good thermal shock resistance
Magnesia fire brick, magnesite chrome brick is detailed as follow :
MgO-Cr2O3 Bricks | |||
MgO | Cr2O3 | Apparent porosity | C.C.S |
(% minm) | (% minm) | (% max) | (MPa minm) |
40 | 20 | 23 | 30 |
45 | 20 | 20 | 35 |
50 | 16 | 20 | 35 |
55 | 12 | 20 | 30 |
60 | 12 | 20 | 35 |
65 | 8 | 20 | 35 |
Recombined MgO-Cr2O3 Bricks | |||
MgO | Cr2O3 | Apparent porosity | C.C.S |
(% minm) | (% minm) | (% max) | (MPa minm) |
50 | 20 | 16 | 40 |
55 | 16 | 16 | 40 |
60 | 20 | 16 | 45 |
65 | 16 | 16 | 45 |
Direct-combined MgO-Cr2O3 Bricks | |||
MgO | Cr2O3 | Apparent porosity | C.C.S |
(% minm) | (% minm) | (% max) | (MPa minm) |
58 | 18 | 18 | 40 |
60 | 16 | 18 | 40 |
65 | 12 | 18 | 40 |
75 | 8 | 18 | 40 |
80 | 4 | 18 | 40 |