Type | Oil ab- sorption |
PH Value of Suspension |
Resi- due of sifting |
Water soluble matter |
Volatile matter at 105℃ |
Masstone (compared with standard) |
Tinting strength (compared with standard) |
Heat resistance |
(g/100g) | / | (45μm mesh, %) |
(%, m/m) | (%, m/m) | % | % | ℃ | |
Iron Oxide Black TX303T |
15-30 | ≥5.0 | ≤0.3 | ≤0.5 | ≤0.5 | ≤1.0 | 95-105 | ≤500 |
Iron Oxide Black TX4330T |
20-40 | 5-8 | ≤0.3 | ≤1.0 | ≤1.0 | ≤1.0 | 95-105 | ≤500 |
Iron Oxide Yellow TX321T |
25-35 | ≥5.0 | ≤0.1 | ≤0.3 | ≤0.5 | ≤1.0 | 95-105 | ≤500, for PP |
Iron Oxide Yellow TXBM810 |
25-35 | ≥5.0 | ≤0.1 | ≤0.4 | ≤0.5 | ≤1.0 | 95-105 | ≤260, for PP |
Iron Oxide Yellow TX4313T |
20-40 | 5-8 | ≤0.3 | ≤1.0 | ≤1.0 | ≤1.0 | 95-105 | ≤500 |
Iron Oxide Blue TX4800T |
20-40 | 5-8 | ≤0.3 | ≤1.0 | ≤1.0 | ≤1.0 | 95-105 | ≤1500 |
Iron Oxide Blue TX4810T |
20-40 | 5-8 | ≤0.3 | ≤1.0 | ≤1.0 | ≤1.0 | 95-105 | ≤1500 |